Concrete slabs will dry at the rate of about 1" per month. So your 6" slab could dry in six months. We used to get those results consistently if we followed the guidelines.

Why is there air in the slab??? Is it outdoors? Subject to freezing?

I really like the LOW cement content of this slab.
When they spec less cement, they also use less water. Less water in = less water to dry out. Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Kapow! Low RH by Sundt - eaadams - 05-06-2013, 09:42 PM
RE: Kapow! Low RH by Sundt - jim decker - 05-07-2013, 06:31 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 06:39 PM
RE: Kapow! Low RH by Sundt - jim decker - 05-07-2013, 06:54 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 07:24 PM
RE: Kapow! Low RH by Sundt - Rubensgt40 - 05-07-2013, 08:38 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 08:40 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-10-2013, 09:36 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-10-2013, 10:14 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-10-2013, 10:22 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-10-2013, 10:26 AM
RE: Kapow! Low RH by Sundt - rapidrhrep - 05-24-2013, 09:41 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-24-2013, 09:48 AM
RE: Kapow! Low RH by Sundt - rapidrhrep - 05-24-2013, 10:09 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-24-2013, 10:16 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-27-2013, 10:17 AM

Users browsing this thread:
1 Guest(s)