(01-16-2012, 08:39 AM)Ernesto Wrote:  Not sure what was so funny about my post. Making cementacious products is not rocket science.

Making cementitious products IS like rocket science! Talk to Tim Murphy at Mineralogy for about 30 minutes..... Or ask Wiss Janney Elstner about the science of cementitious underlayments and overlays.

Did you know that only two people know the recipe for K15? Do you know how many people have tried to copy K15 and Feather Finish over the last 20-30 years?

It's not rocket science, but it's as close as you can get. Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
I think the economy is improving - eaadams - 01-14-2012, 02:18 AM
RE: I think the economy is improving - CC Solutions - 01-14-2012, 09:23 AM
RE: I think the economy is improving - Ernesto - 01-14-2012, 03:50 PM
RE: I think the economy is improving - CC Solutions - 01-15-2012, 09:20 AM
RE: I think the economy is improving - Ernesto - 01-15-2012, 10:43 AM
RE: I think the economy is improving - CC Solutions - 01-15-2012, 11:04 AM
RE: I think the economy is improving - CCR - 01-15-2012, 02:02 PM
RE: I think the economy is improving - Ernesto - 01-15-2012, 04:32 PM
RE: I think the economy is improving - Ernesto - 01-15-2012, 06:04 PM
RE: I think the economy is improving - CC Solutions - 01-15-2012, 06:18 PM
RE: I think the economy is improving - Rubensgt40 - 01-15-2012, 06:38 PM
RE: I think the economy is improving - Ernesto - 01-16-2012, 08:39 AM
RE: I think the economy is improving - CC Solutions - 01-17-2012, 07:38 AM
RE: I think the economy is improving - Ernesto - 01-17-2012, 05:45 PM
RE: I think the economy is improving - CC Solutions - 01-17-2012, 07:50 PM
RE: I think the economy is improving - Ernesto - 01-19-2012, 02:44 PM
RE: I think the economy is improving - CC Solutions - 01-19-2012, 03:06 PM
RE: I think the economy is improving - Ernesto - 01-19-2012, 07:38 PM
RE: I think the economy is improving - CC Solutions - 01-19-2012, 08:30 PM
RE: I think the economy is improving - Ernesto - 01-20-2012, 04:20 PM
RE: I think the economy is improving - eaadams - 03-27-2012, 09:32 AM
RE: I think the economy is improving - CC Solutions - 03-27-2012, 09:51 AM
RE: I think the economy is improving - CCR - 03-27-2012, 06:01 PM
RE: I think the economy is improving - CC Solutions - 03-27-2012, 08:01 PM
RE: I think the economy is improving - CCR - 03-27-2012, 09:48 PM
RE: I think the economy is improving - CC Solutions - 03-28-2012, 06:07 AM
RE: I think the economy is improving - eaadams - 04-25-2012, 12:26 PM
RE: I think the economy is improving - CC Solutions - 04-25-2012, 01:17 PM

Users browsing this thread:
1 Guest(s)