I have high expectations for 2012. Just finished an Elite Crete Systems Seminar and going to start doing concrete overlays, epoxy coatings and concrete restoration overlays.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
I think the economy is improving - eaadams - 01-14-2012, 02:18 AM
RE: I think the economy is improving - CC Solutions - 01-14-2012, 09:23 AM
RE: I think the economy is improving - Ernesto - 01-14-2012, 03:50 PM
RE: I think the economy is improving - CC Solutions - 01-15-2012, 09:20 AM
RE: I think the economy is improving - Ernesto - 01-15-2012, 10:43 AM
RE: I think the economy is improving - CC Solutions - 01-15-2012, 11:04 AM
RE: I think the economy is improving - CCR - 01-15-2012, 02:02 PM
RE: I think the economy is improving - Ernesto - 01-15-2012, 04:32 PM
RE: I think the economy is improving - Ernesto - 01-15-2012, 06:04 PM
RE: I think the economy is improving - CC Solutions - 01-15-2012, 06:18 PM
RE: I think the economy is improving - Rubensgt40 - 01-15-2012, 06:38 PM
RE: I think the economy is improving - Ernesto - 01-16-2012, 08:39 AM
RE: I think the economy is improving - CC Solutions - 01-17-2012, 07:38 AM
RE: I think the economy is improving - Ernesto - 01-17-2012, 05:45 PM
RE: I think the economy is improving - CC Solutions - 01-17-2012, 07:50 PM
RE: I think the economy is improving - Ernesto - 01-19-2012, 02:44 PM
RE: I think the economy is improving - CC Solutions - 01-19-2012, 03:06 PM
RE: I think the economy is improving - Ernesto - 01-19-2012, 07:38 PM
RE: I think the economy is improving - CC Solutions - 01-19-2012, 08:30 PM
RE: I think the economy is improving - Ernesto - 01-20-2012, 04:20 PM
RE: I think the economy is improving - eaadams - 03-27-2012, 09:32 AM
RE: I think the economy is improving - CC Solutions - 03-27-2012, 09:51 AM
RE: I think the economy is improving - CCR - 03-27-2012, 06:01 PM
RE: I think the economy is improving - CC Solutions - 03-27-2012, 08:01 PM
RE: I think the economy is improving - CCR - 03-27-2012, 09:48 PM
RE: I think the economy is improving - CC Solutions - 03-28-2012, 06:07 AM
RE: I think the economy is improving - eaadams - 04-25-2012, 12:26 PM
RE: I think the economy is improving - CC Solutions - 04-25-2012, 01:17 PM

Users browsing this thread:
2 Guest(s)