Just realized I was in a hurry to get a job done and had the slab tested by my favorite 3rd party ICRI Wagner RH tester.

The GC took the testing out of my scope in our contract. I din't catch that.

Now I am down $1250 for 10 probes of testing.

Wish this had happened on Monday not today. Sad

Finishing off this crap week strong! Angry

05-31-2013, 05:16 PM #2
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
The GC should do right by you, since it sounds like he got something for nothing!

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

06-28-2013, 10:29 AM #3
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
He met me part way, $750.

So not a total loss. Will have to see if he pays

06-30-2013, 04:21 PM #4
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Hey, at $75 a pop, at least you covered your costs and made $7.48.Big Grin That's about what I made on my first long distance testing job. LOL

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

07-02-2013, 08:33 AM #5
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
You guys mean you MAKE MONEY testing???? Huh

I KNEW I was doing something wrong..... Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

07-02-2013, 09:46 AM #6
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
I made $7.23 onceBig Grin

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

07-02-2013, 10:03 AM #7
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
What is minimum wage now? $7.35

07-02-2013, 12:03 PM #8
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Yup. And I'm gonna sue myself for the underpaymentBig Grin

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

07-02-2013, 05:55 PM #9
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
(07-02-2013, 08:33 AM)CC Solutions Wrote:  You guys mean you MAKE MONEY testing???? Huh

I KNEW I was doing something wrong..... Big Grin

Stop SCARING me...!

Of COURSE you can make money testing..

(Clicks heels together..there's no place like home...there's no place like home...)

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher









Possibly Related Threads...
Thread / Author Replies / Views Last Post

Users browsing this thread:
1 Guest(s)