... today I learned to look at other parts of the concrete design. The slab design said 5". But, one side of the gym came in at 99%.

I freaked out and said oh no oh no henny penny the sky is falling. I now feel pretty dumb.

After some research the GC pointed out that the side of the gym that is reading high has a masonry wall. On that side of the room, the concrete is 14" thick to support the masonry wall. So duh it isn't dry.

Anyway, I have to figure out how to read walls now before bid. Not sure how but I will have to pull out this projects plans and teach myself a new skill.

Learn something new every day. Shows why we have GC's. They do have the whole building in mind. Smile

Now I have to find out if the sealing company can do the whole bead blast and seal and top coat 12' of concrete without having to level the whole floor.








Messages In This Thread
I learned something new today... - eaadams - 11-02-2011, 09:09 PM
RE: I learned something new today... - CC Solutions - 11-03-2011, 06:50 AM

Users browsing this thread:
1 Guest(s)