(11-06-2013, 04:33 PM)Ernesto Wrote:  Hope those gas heaters are not propane. The exaust from propane has a high moisture content.

Yes it does! So does kerosene which you see as the white trails left in the sky by jets. It's moisture freezing in the cold dry air up there.

Temporary heaters also tend to contribute to elevated CO levels, increasing the carbonation at the concrete surface. I had a couple projects that had so much carbonated concrete due to unvented temporary heat that the concrete surface was soft and easily scratched with a pocket knife.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
How do I get my concrete to cure faster! - Avcraft - 08-18-2013, 08:21 PM
RE: How do I get my concrete to cure faster! - rapidrhrep - 08-20-2013, 11:43 AM
RE: How do I get my concrete to cure faster! - Avcraft - 08-20-2013, 04:37 PM
RE: How do I get my concrete to cure faster! - CC Solutions - 09-01-2013, 08:44 AM
RE: How do I get my concrete to cure faster! - Ernesto - 11-06-2013, 04:33 PM
RE: How do I get my concrete to cure faster! - CC Solutions - 12-04-2013, 08:46 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post

Users browsing this thread:
1 Guest(s)