08-19-2011, 09:00 PM #9
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Definition? It's a crack. Big, but a crack. If it moves, oh well! Either you can honor it through or hope it is stable. I'd prefer the later, you can always cut a nice joint in the finished floor.

Fill it with cement, epoxy over it to seal it well, and put flooring on it. It will hold up. Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
How are you addressing cracks? - CC Solutions - 08-11-2011, 08:03 AM
RE: How are you addressing cracks? - Ernesto - 08-14-2011, 08:16 PM
RE: How are you addressing cracks? - CC Solutions - 08-14-2011, 09:34 PM
RE: How are you addressing cracks? - eaadams - 08-19-2011, 03:56 PM
RE: How are you addressing cracks? - CC Solutions - 08-19-2011, 04:20 PM
RE: How are you addressing cracks? - Ernesto - 08-19-2011, 08:17 PM
RE: How are you addressing cracks? - CC Solutions - 08-19-2011, 08:26 PM
RE: How are you addressing cracks? - Ernesto - 08-19-2011, 08:32 PM
RE: How are you addressing cracks? - CC Solutions - 08-19-2011, 09:00 PM
RE: How are you addressing cracks? - Ernesto - 08-20-2011, 06:40 AM
RE: How are you addressing cracks? - CC Solutions - 08-20-2011, 09:51 PM
RE: How are you addressing cracks? - Ernesto - 08-25-2011, 06:53 PM
RE: How are you addressing cracks? - rthompson - 08-26-2011, 01:55 PM
RE: How are you addressing cracks? - CC Solutions - 08-26-2011, 02:30 PM
RE: How are you addressing cracks? - eaadams - 08-31-2011, 11:53 AM
RE: How are you addressing cracks? - rthompson - 08-31-2011, 01:17 PM
RE: How are you addressing cracks? - CC Solutions - 08-31-2011, 02:54 PM
RE: How are you addressing cracks? - eaadams - 09-14-2011, 01:26 AM
RE: How are you addressing cracks? - CC Solutions - 09-14-2011, 07:07 AM
RE: How are you addressing cracks? - eaadams - 09-14-2011, 06:41 PM
RE: How are you addressing cracks? - Ernesto - 09-14-2011, 07:09 PM
RE: How are you addressing cracks? - CC Solutions - 09-15-2011, 05:40 AM
RE: How are you addressing cracks? - eaadams - 09-15-2011, 12:06 PM
RE: How are you addressing cracks? - CC Solutions - 09-15-2011, 01:10 PM
RE: How are you addressing cracks? - Ernesto - 09-20-2011, 08:14 PM
RE: How are you addressing cracks? - CC Solutions - 09-20-2011, 08:29 PM
RE: How are you addressing cracks? - eaadams - 10-19-2011, 09:55 PM
RE: How are you addressing cracks? - CC Solutions - 10-20-2011, 06:58 AM
RE: How are you addressing cracks? - rthompson - 10-20-2011, 09:38 AM
RE: How are you addressing cracks? - eaadams - 10-20-2011, 05:07 PM
RE: How are you addressing cracks? - Ernesto - 10-20-2011, 07:17 PM
RE: How are you addressing cracks? - CC Solutions - 10-21-2011, 07:02 AM
RE: How are you addressing cracks? - eaadams - 10-21-2011, 09:20 AM

Users browsing this thread:
1 Guest(s)