You had three 'no-tests' on 8/7. It would help to see what those probes read.

Were the probes acclimated for 72 hours on the first test date of 7/11? If not we should discount those readings.

When the slab temp rises we expect to see a decrease in relative humidity. Additional readings would help indicate a trend. Another helpful bit of information would be ambient conditions and whether the HVAC is constantly on or just being run sporadically. Is the building envelope completed and sealed?

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Heat, move air, shotblast = lower results - eaadams - 08-07-2013, 12:35 PM
RE: Heat, move air, shotblast = lower results - CC Solutions - 09-01-2013, 07:56 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
7 Replies 21,565 Views
Last Post by Rubensgt40
05-09-2012, 04:35 PM
11 Replies 32,397 Views
Last Post by CC Solutions
10-28-2011, 02:12 PM

Users browsing this thread:
1 Guest(s)