I hope they trust your testing and you can explain why and how your results are what they are.

The adhesives used today are really some of the best ever produced. I am amazed at how well they work, even when conditions aren't anywhere close to what they should be.

I understand how a company can forego testing and still have a great percentage of success. But with accurate testing I know that same company will dramatically reduce the possibility of failures due to moisture and alkalinity.

In other words, by spending a few dollars conducting good RH testing, the flooring installer dramatically reduces their risk exposure.

That's money in the bank! Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
First Test - Ever - CCR - 08-30-2013, 12:11 PM
RE: First Test - Ever - CC Solutions - 09-01-2013, 07:48 AM
RE: First Test - Ever - CCR - 09-01-2013, 12:29 PM
RE: First Test - Ever - Rubensgt40 - 09-01-2013, 04:38 PM
RE: First Test - Ever - CCR - 09-01-2013, 06:04 PM
RE: First Test - Ever - Ernesto - 01-16-2014, 07:45 PM
RE: First Test - Ever - eaadams - 01-30-2014, 12:23 AM

Users browsing this thread:
1 Guest(s)