09-10-2013, 07:13 PM #6
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Thats the problem, no one agrees on every testing procedure. This moisture testing of concrete is...has always been full of crazy hypotheses.

Hedenblad's study was based on new concrete. tHIS IS THE BASIS FOR ASTM F 2170-11. What about old concrete? Does it apply? No one ever speaks of old CC. Thats mostly where I'm at is with old concrete. A whole different animal.

Anyone who hires a moisture abatement guy to test his new slab is an idiot. Call me TAINTED. LOL

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
F1869's Grandfather - CCR - 08-06-2013, 11:08 AM
RE: F1869's Grandfather - Ernesto - 08-06-2013, 08:32 PM
RE: F1869's Grandfather - CCR - 08-28-2013, 09:25 AM
RE: F1869's Grandfather - eaadams - 08-29-2013, 10:41 AM
RE: F1869's Grandfather - CC Solutions - 09-01-2013, 07:42 AM
RE: F1869's Grandfather - Ernesto - 09-10-2013, 07:13 PM

Users browsing this thread:
2 Guest(s)