If the slab is open, it will pull moisture out of the surface. Doesn't do much for moisture in the slab. My theory is removing the moisture near the surface will speed the process. gene








Messages In This Thread
Epoxy over 7 day old slab - ec-Indy - 08-18-2011, 03:08 PM
RE: Epoxy over 7 day old slab - Ernesto - 08-18-2011, 07:30 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-18-2011, 10:29 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-19-2011, 07:07 AM
RE: Epoxy over 7 day old slab - Ernesto - 08-19-2011, 08:00 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-19-2011, 08:21 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-20-2011, 12:48 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-20-2011, 09:47 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-21-2011, 02:26 AM
RE: Epoxy over 7 day old slab - CC Solutions - 08-21-2011, 08:06 AM
RE: Epoxy over 7 day old slab - ec-Indy - 08-21-2011, 08:13 AM
RE: Epoxy over 7 day old slab - eaadams - 08-25-2011, 11:01 AM
RE: Epoxy over 7 day old slab - CC Solutions - 08-25-2011, 04:39 PM
RE: Epoxy over 7 day old slab - rthompson - 08-26-2011, 02:03 PM

Users browsing this thread:
1 Guest(s)