(07-19-2013, 05:10 PM)CCR Wrote:  Never checked with Jason, but I can tell you it dries pretty fast and hard. I don't think it has an effect on final readings because I have seen readings go up, down and remain the same as my initial readings, depending on the slab conditions. Besides, it stands to reason (to me anyway) that like MVE, any moisture given off is going up into the air more than down into the sensor. I started doing this after my first few tests when I started when I experienced a lot of contamination getting into my sensors. Even had a bunch destroyed on a job when the GC scheduled wet saw cutting in slabs during the test cycle (grrrrr).

JD...now you have me wondering about the moisture given off by the sealant. Perhaps a urethane would be better. All I know is I have found sealing necessary due to the contamination issues, as well as (unfortunately) the lack of "respect" of the test locations sometimes by workers during the test period. I even surround each location with strips of bright orange tape labeled "Please Do Not Disturb" which helps considerably.

Would be great to have Jason chime in on this one!!!

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
Debris in the Sensor - Ernesto - 10-03-2011, 01:18 PM
RE: Debris in the Sensor - CC Solutions - 10-03-2011, 04:06 PM
RE: Debris in the Sensor - Ernesto - 10-04-2011, 02:13 PM
RE: Debris in the Sensor - CC Solutions - 10-04-2011, 02:52 PM
RE: Debris in the Sensor - Ernesto - 10-04-2011, 03:23 PM
RE: Debris in the Sensor - CC Solutions - 10-04-2011, 03:56 PM
RE: Debris in the Sensor - Ernesto - 10-04-2011, 06:04 PM
RE: Debris in the Sensor - CC Solutions - 10-06-2011, 11:31 AM
RE: Debris in the Sensor - Ernesto - 10-06-2011, 03:40 PM
RE: Debris in the Sensor - CCR - 07-19-2013, 04:21 PM
RE: Debris in the Sensor - CC Solutions - 07-19-2013, 04:41 PM
RE: Debris in the Sensor - CCR - 07-19-2013, 05:10 PM
RE: Debris in the Sensor - CCR - 07-20-2013, 04:54 AM
RE: Debris in the Sensor - CC Solutions - 07-22-2013, 09:09 AM
RE: Debris in the Sensor - CCR - 07-22-2013, 12:10 PM
RE: Debris in the Sensor - rapidrhrep - 07-23-2013, 11:11 AM
RE: Debris in the Sensor - CCR - 07-23-2013, 11:30 AM
RE: Debris in the Sensor - CC Solutions - 07-23-2013, 08:36 PM
RE: Debris in the Sensor - rapidrhrep - 07-23-2013, 08:46 PM
RE: Debris in the Sensor - CC Solutions - 07-23-2013, 08:48 PM
RE: Debris in the Sensor - rapidrhrep - 07-23-2013, 08:55 PM
RE: Debris in the Sensor - CCR - 07-24-2013, 08:15 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
1 Replies 10,333 Views
Last Post by rthompson
10-01-2008, 03:46 PM

Users browsing this thread:
1 Guest(s)