Cork is a great floor do a lot of US Floors never a problem. Years ago when I did all of Dartmouth Colleges floor work in NH. I replaced a cork floor in the administration building that had been down 50 years didn't look bad replaced with nylon commercial carpet.
Beware of click wood or cork if the house cannot maintain the relative humidity requirements of the cork mfg. Particularly in arid areas if they shrink somewhat as they then may make clicking noises.








Messages In This Thread
Cork flooring - CC Solutions - 12-01-2012, 09:37 AM
RE: Cork flooring - CCR - 12-01-2012, 11:55 AM
RE: Cork flooring - Ernesto - 12-01-2012, 05:25 PM
RE: Cork flooring - CC Solutions - 12-01-2012, 06:52 PM
RE: Cork flooring - CCR - 12-02-2012, 10:21 AM
RE: Cork flooring - Rubensgt40 - 12-02-2012, 03:00 PM
RE: Cork flooring - CC Solutions - 12-03-2012, 01:32 PM
RE: Cork flooring - eaadams - 12-03-2012, 02:06 PM
RE: Cork flooring - CCR - 12-03-2012, 03:15 PM
RE: Cork flooring - Rubensgt40 - 12-03-2012, 06:55 PM
RE: Cork flooring - CC Solutions - 12-04-2012, 10:41 AM
RE: Cork flooring - Ernesto - 12-04-2012, 08:40 PM
RE: Cork flooring - CC Solutions - 12-05-2012, 07:46 AM
RE: Cork flooring - CC Solutions - 12-07-2012, 07:18 PM
RE: Cork flooring - CCR - 12-09-2012, 05:55 AM
RE: Cork flooring - CC Solutions - 12-09-2012, 09:42 AM
RE: Cork flooring - CCR - 12-09-2012, 10:19 AM
RE: Cork flooring - CC Solutions - 12-09-2012, 10:42 AM
RE: Cork flooring - CCR - 12-09-2012, 11:11 AM
RE: Cork flooring - CC Solutions - 12-20-2012, 09:38 PM
RE: Cork flooring - CCR - 12-21-2012, 07:20 AM
RE: Cork flooring - CC Solutions - 12-21-2012, 08:40 AM
RE: Cork flooring - CCR - 12-21-2012, 09:11 AM
RE: Cork flooring - CC Solutions - 12-21-2012, 10:05 AM
RE: Cork flooring - eaadams - 12-22-2012, 11:49 AM
RE: Cork flooring - CC Solutions - 12-22-2012, 03:07 PM
RE: Cork flooring - jim decker - 04-29-2013, 08:36 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post

Users browsing this thread:
1 Guest(s)