Cork is much more muffled. Before you install assemble several planks and walk on them to get a feel for the sound and if you want to go the step by installing the sheet cushion. Wonder if anybody else has suggestions

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
Cork flooring - CC Solutions - 12-01-2012, 09:37 AM
RE: Cork flooring - CCR - 12-01-2012, 11:55 AM
RE: Cork flooring - Ernesto - 12-01-2012, 05:25 PM
RE: Cork flooring - CC Solutions - 12-01-2012, 06:52 PM
RE: Cork flooring - CCR - 12-02-2012, 10:21 AM
RE: Cork flooring - Rubensgt40 - 12-02-2012, 03:00 PM
RE: Cork flooring - CC Solutions - 12-03-2012, 01:32 PM
RE: Cork flooring - eaadams - 12-03-2012, 02:06 PM
RE: Cork flooring - CCR - 12-03-2012, 03:15 PM
RE: Cork flooring - Rubensgt40 - 12-03-2012, 06:55 PM
RE: Cork flooring - CC Solutions - 12-04-2012, 10:41 AM
RE: Cork flooring - Ernesto - 12-04-2012, 08:40 PM
RE: Cork flooring - CC Solutions - 12-05-2012, 07:46 AM
RE: Cork flooring - CC Solutions - 12-07-2012, 07:18 PM
RE: Cork flooring - CCR - 12-09-2012, 05:55 AM
RE: Cork flooring - CC Solutions - 12-09-2012, 09:42 AM
RE: Cork flooring - CCR - 12-09-2012, 10:19 AM
RE: Cork flooring - CC Solutions - 12-09-2012, 10:42 AM
RE: Cork flooring - CCR - 12-09-2012, 11:11 AM
RE: Cork flooring - CC Solutions - 12-20-2012, 09:38 PM
RE: Cork flooring - CCR - 12-21-2012, 07:20 AM
RE: Cork flooring - CC Solutions - 12-21-2012, 08:40 AM
RE: Cork flooring - CCR - 12-21-2012, 09:11 AM
RE: Cork flooring - CC Solutions - 12-21-2012, 10:05 AM
RE: Cork flooring - eaadams - 12-22-2012, 11:49 AM
RE: Cork flooring - CC Solutions - 12-22-2012, 03:07 PM
RE: Cork flooring - jim decker - 04-29-2013, 08:36 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post

Users browsing this thread:
1 Guest(s)