#Login Register
Condensation
  • 0 Vote(s) - 0 Average


10-04-2013, 01:38 PM #1
eaadams Concrete Moisture Expert *****
Status: Offline Posts:596 Threads:86 Joined:Jul 2010
I was watching a competitor to Wagner's youtube today. It talked about how 'throw away' probes 'max out' due to condensation.

Any comment?

How would one know if they have a condensation issue with probes on RH tests that sit for extended periods of time (weeks to months)?

10-09-2013, 09:14 AM #2
rapidrhrep Concrete Moisture Tutor **
Status: Offline Posts:83 Threads:3 Joined:Aug 2011
EA:

I hope all is well. The "issue" the competitor is trying to bring up is one that we have discussed in the thread below. Let me know if you need any additional information.

Jason

http://www.wagnermeters.com/concreteforum/Thread-Relative-Humidity-Hysteresis?pid=3199&highlight=hyster#pid3199