Ray that is not my point. I'm not looking at removing a surface.

I'm talking about the smoothness needed for resilient sheet flooring. A CSP of 3-4 would need to be re surfaced to put flooring on.

06-21-2011, 11:42 AM #12
rthompson Industry Expert *****
Status: Offline Posts:72 Threads:0 Joined:Sep 2008
Concrete should have the texture of about 100 grit sandpaper to obtain a good mechanical bond for sheet vinyl adhesives and especially epoxies. Burnished concrete not only compromises adhesive bond, but retards the moisture drying in a timely fashion. If the moisture is there it is going to get out eventually.
Regards
Rayt

06-21-2011, 11:47 AM #13
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
Agreed Ray. The big issue is open and porous, and sandpaper type texture is an easy reference. Sandpaper is everywhere.

Looking back over the posts, that CC Solutions guy has some good info on this thread... Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 7,294 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 18,563 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 34,373 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 83,108 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 11,555 Views
Last Post by eaadams
01-30-2013, 04:43 PM
32 Replies 76,917 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 4,704 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 62,657 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
8 Replies 21,515 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
1 Guest(s)