Cold Expansion Joint
  • 0 Vote(s) - 0 Average


08-15-2011, 04:04 AM #11
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
Sometimes it works out to be the best. I lose jobs every day because people don't want to do it right. Sad

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

08-16-2011, 08:11 PM #12
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Doin it right is cheaper than crossing fingers.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

08-19-2011, 07:14 AM #13
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
(08-16-2011, 08:11 PM)Ernesto Wrote:  Doin it right is cheaper than crossing fingers.

I may steal that line.... I like it a lot! Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

10-21-2011, 06:53 PM #14
eaadams Concrete Moisture Expert *****
Status: Online Posts:596 Threads:86 Joined:Jul 2010
Jd you mentioned the euco quikjoint 200. Perhaps you know the other products.

I have a job where GC put euco 700 in a stress crack (poorly spaced joints) running the whole width of slab 80'.

Now we can see a line tracking the crack repair under the flooring. Does that jive in your mind?

I am having a hard time understanding the difference between them.

10-21-2011, 07:30 PM #15
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
(10-21-2011, 06:53 PM)eaadams Wrote:  Jd you mentioned the euco quikjoint 200. Perhaps you know the other products.

I have a job where GC put euco 700 in a stress crack (poorly spaced joints) running the whole width of slab 80'.

Now we can see a line tracking the crack repair under the flooring. Does that jive in your mind?

I am having a hard time understanding the difference between them.

Understanding the difference between what?

If you see a crack, the joint has moved. Why else would you see the crack?

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

10-21-2011, 07:49 PM #16
eaadams Concrete Moisture Expert *****
Status: Online Posts:596 Threads:86 Joined:Jul 2010
Between why the structural engineer would spec a epoxy euco 700 vs the polyurea euco 200.

When I read about the two it seems to say the.same thing.

10-22-2011, 07:24 AM #17
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
The 700 is an epoxy and harder. Has a longer open time and would flow to the bottom of the crack better.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com