Perhaps you misunderstand my position on carbide testing....

It is a soils test being spec'd by silicate pushers because they think they can fool people into believing it means something.

The way they are testing means nothing to anyone in the flooring industry.

As for CaCl testing, it is nearly worthless for determining the potential a floor has for failure. I'd rather put in 5 Wagners at a cost of $200 (including installation and reading) than 7 CaCl tests for the same cost, when the CaCl tests tell you nothing about the condition of the slab, and the results are unreliable.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Carbide moisture testing - CC Solutions - 09-18-2012, 10:19 AM
RE: Carbide moisture testing - eaadams - 09-18-2012, 11:01 AM
RE: Carbide moisture testing - CC Solutions - 09-18-2012, 12:25 PM
RE: Carbide moisture testing - eaadams - 09-18-2012, 02:02 PM
RE: Carbide moisture testing - CC Solutions - 09-18-2012, 06:11 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 5,503 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
4 Replies 7,237 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 18,423 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 4,958 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 7,385 Views
Last Post by eaadams
09-27-2013, 10:26 AM
33 Replies 64,709 Views
Last Post by eaadams
11-21-2012, 10:19 AM
51 Replies 110,409 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
22 Replies 44,562 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
23 Replies 62,554 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 14,265 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)