Calcium Carbide testing and Silicates
  • 0 Vote(s) - 0 Average


11-16-2012, 01:52 AM #37
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
(11-15-2012, 10:47 AM)ILLENTINC Wrote:  Of course the adhesive/mitigation manufacturers are highly dismissive of it. It is a competitive product to the standard mitigation systems. When QUALITY products of this nature are PROPERLY used, there is no need for the several dollar a square foot mitigation systems. Do you really think the mitigation manufacturers are going to sing the praises of such a product?

An adhesive is the manufacturer's bread and butter- you need it whether the slab is wet or not. They can live without selling mitigation systems. They need to know that a product is not going to cause their adhesive to fail, and it's not their responsibility to put the R & D into it. By the way, the silicate-based product I'm talking about is as pricey and in some cases more expensive that "standard mitigation systems".

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher









Messages In This Thread
Calcium Carbide testing and Silicates - Lepito - 09-15-2012, 08:12 AM
RE: Calcium Carbide testing and Silicates - eaadams - 09-15-2012, 09:04 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-15-2012, 11:38 AM
RE: Calcium Carbide testing and Silicates - eaadams - 09-15-2012, 12:32 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-15-2012, 02:00 PM
RE: Calcium Carbide testing and Silicates - Lepito - 09-15-2012, 06:13 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 09-16-2012, 06:34 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-16-2012, 09:15 PM
RE: Calcium Carbide testing and Silicates - eaadams - 09-16-2012, 10:50 PM
RE: Calcium Carbide testing and Silicates - Lepito - 09-17-2012, 07:38 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-18-2012, 07:47 AM
RE: Calcium Carbide testing and Silicates - Concrete1421 - 09-18-2012, 12:40 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-18-2012, 06:03 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 09-18-2012, 10:58 PM
RE: Calcium Carbide testing and Silicates - Lepito - 09-19-2012, 06:40 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-19-2012, 06:59 AM
RE: Calcium Carbide testing and Silicates - Lepito - 09-19-2012, 07:01 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-20-2012, 05:41 AM
RE: Calcium Carbide testing and Silicates - eaadams - 09-24-2012, 10:00 AM
RE: Calcium Carbide testing and Silicates - Newenglandci - 09-24-2012, 10:51 AM
RE: Calcium Carbide testing and Silicates - Newenglandci - 09-24-2012, 02:12 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 09-24-2012, 03:59 PM
RE: Calcium Carbide testing and Silicates - Specsystems - 09-27-2012, 10:41 AM
RE: Calcium Carbide testing and Silicates - eaadams - 10-15-2012, 03:47 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 10-15-2012, 03:54 PM
RE: Calcium Carbide testing and Silicates - eaadams - 10-15-2012, 04:38 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 10-15-2012, 06:12 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 10-15-2012, 08:04 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 10-15-2012, 08:34 PM
RE: Calcium Carbide testing and Silicates - Ernesto - 10-16-2012, 01:59 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 10-21-2012, 04:34 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-15-2012, 10:47 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-15-2012, 12:49 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-15-2012, 02:13 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-15-2012, 02:27 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-15-2012, 02:37 PM
RE: Calcium Carbide testing and Silicates - Rubensgt40 - 11-16-2012, 01:52 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 07:03 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-16-2012, 07:08 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 07:59 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-16-2012, 09:03 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 09:19 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-16-2012, 09:27 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 01:54 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-16-2012, 03:06 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-16-2012, 11:10 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-17-2012, 06:22 PM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-18-2012, 08:41 PM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-19-2012, 08:33 AM
RE: Calcium Carbide testing and Silicates - eaadams - 11-19-2012, 11:36 AM
RE: Calcium Carbide testing and Silicates - CC Solutions - 11-19-2012, 11:56 AM
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-19-2012, 11:59 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 8,196 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
2 Replies 8,026 Views
Last Post by eaadams
09-27-2013, 10:26 AM
33 Replies 69,207 Views
Last Post by eaadams
11-21-2012, 10:19 AM
4 Replies 12,759 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 47,302 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
36 Replies 88,770 Views
Last Post by CC Solutions
04-19-2011, 04:59 PM
9 Replies 26,888 Views
Last Post by CC Solutions
04-05-2011, 05:33 AM
2 Replies 10,963 Views
Last Post by eaadams
09-30-2010, 08:27 AM
11 Replies 33,944 Views
Last Post by CC Solutions
09-20-2010, 03:01 PM
11 Replies 33,279 Views
Last Post by CC Solutions
05-11-2010, 03:22 PM

Users browsing this thread:
1 Guest(s)