So do you test at the standing temp in the room, 85deg or at the high point in the room 105deg (hits 105 during classes but then they ramp down)

10-15-2013, 08:05 PM #2
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
That's a bewdy.

When F2170 said "service conditions" they may not have considered a Yoga class...

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher


10-23-2013, 01:28 PM #3
eaadams Concrete Moisture Expert *****
Status: Offline Posts:596 Threads:86 Joined:Jul 2010
Something I just realized. Often when we do a gym in California we will install at 80 but in the summer when the kids go home the room can easily get into the 100-115 range.