I've poured about 1000 bags of Ardex V1200 over the last month and I am really beginning to like it!!

We poured 100 bags on a job where two slab elevations were off and I ended up putting the V1200 in 2 1/2" thick (two lifts) and I was pleased to find ZERO cracking and a perfect finish.

We pumped in about 600 bags on a retail floor with some low areas and some feathering to nothing and it flows nice, heals nice and finishes nice. Very consistent! No surprises when it's warm in a building or cool. We've mixed with differing water temps and it always flows nicely.

Pricing is pretty good too if you buy in quantity.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Ardex V1200 - CC Solutions - 03-27-2012, 09:57 AM
RE: Ardex V1200 - eaadams - 03-27-2012, 10:03 AM
RE: Ardex V1200 - CC Solutions - 03-27-2012, 10:36 AM
RE: Ardex V1200 - eaadams - 04-25-2012, 02:01 PM
RE: Ardex V1200 - CC Solutions - 04-25-2012, 04:06 PM
RE: Ardex V1200 - CCR - 04-26-2012, 04:36 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 06:11 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:11 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:18 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:33 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:16 PM
RE: Ardex V1200 - eaadams - 04-26-2012, 08:36 PM
RE: Ardex V1200 - CC Solutions - 04-27-2012, 06:06 AM
RE: Ardex V1200 - eaadams - 05-07-2012, 09:45 AM
RE: Ardex V1200 - CC Solutions - 05-07-2012, 12:27 PM
RE: Ardex V1200 - eaadams - 07-10-2012, 10:28 AM
RE: Ardex V1200 - CCR - 07-10-2012, 11:40 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 06:19 AM
RE: Ardex V1200 - CCR - 07-12-2012, 07:49 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 08:10 AM
RE: Ardex V1200 - eaadams - 07-12-2012, 12:56 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:33 PM
RE: Ardex V1200 - eaadams - 07-12-2012, 01:42 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:50 PM
RE: Ardex V1200 - CCR - 07-12-2012, 02:46 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 04:25 PM

Users browsing this thread:
1 Guest(s)