The system used to fix this project was from Ardex.


(08-30-2013 12:11 PM)eaadams Wrote:  
(08-07-2013 08:10 AM)eaadams Wrote:  heh ... talk to me after next Friday. Smile 40,000 sf up to bid.

I have a CTL spec here from another project where the beadblast was enough. But not sure in the new job what the new rules will be.

I will say I got an ear full from George Donnelly last week. Some of my ideas about unreacted lithium silicates that Harold / Minerology would say he takes great objection to.

Ardex came out with a much better spec to fix these slabs with MC Ultra. But looks like I lost the jobs to someone who is going to risk it with MC Rapid against some peoples explicit warnings not to use it.

(08-30-2013 01:08 PM)eaadams Wrote:  Yea that is why I went with Mr Level Master Elite and the others .... didn't.

Dice, they've got six sides. Perhaps they will get lucky.

I sense a failure on the horizon, not even knowing all the details

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Visit this user's website Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Amazing Concrete Moisture Solution! - CCR - 05-30-2013, 05:33 PM
RE: Amazing Concrete Moisture Solution! - CCR - 08-30-2013 01:09 PM