A little tidbit I found in some lit:

302.2R-18 ACI COMMITTEE REPORT

"shown that the adhesive strength decreases with an increase
in the concrete’s MVER. When these tests were conducted,
however, there were no criteria for acceptable bond strength,
and scatter in the test results did not indicate a clear dividing line
between acceptable and nonacceptable adhesive bond strength.
A report on recent testing that attempted to correlate moisture
in the concrete with floor covering performance concluded
that: “The evidence presented suggests that there is no
relationship between the relative humidity of a concrete base
or screed and adhesion of resilient floor coverings” (The
Concrete Society 2004).
While moisture criteria are often used, the relationship
between these criteria and floor covering performance is not
well understood."








Messages In This Thread
Adhesives and Moisture - Ernesto - 02-03-2010, 01:41 PM
RE: Adhesives and Moisture - CC Solutions - 02-03-2010, 03:53 PM
RE: Adhesives and Moisture - Ernesto - 02-05-2010, 08:12 AM
RE: Adhesives and Moisture - CC Solutions - 02-05-2010, 11:56 AM
RE: Adhesives and Moisture - Ernesto - 02-17-2010, 03:32 PM
RE: Adhesives and Moisture - CC Solutions - 02-17-2010, 10:12 PM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 09:04 AM
RE: Adhesives and Moisture - CC Solutions - 02-18-2010, 09:34 AM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 03:19 PM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 07:13 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 08:34 AM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 11:07 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 05:31 PM
RE: Adhesives and Moisture - Ernesto - 03-08-2010, 03:11 PM
RE: Adhesives and Moisture - CC Solutions - 03-09-2010, 06:48 PM
RE: Adhesives and Moisture - Ernesto - 03-10-2010, 03:06 PM
RE: Adhesives and Moisture - CC Solutions - 03-18-2010, 06:31 PM
RE: Adhesives and Moisture - Ernesto - 03-19-2010, 06:01 PM
RE: Adhesives and Moisture - tbrown - 04-08-2010, 10:24 AM
RE: Adhesives and Moisture - CC Solutions - 04-08-2010, 08:10 PM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 04-29-2010, 08:38 AM
RE: Adhesives and Moisture - CC Solutions - 04-30-2010, 09:03 AM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 04-30-2010, 09:33 AM
RE: Adhesives and Moisture - CC Solutions - 05-01-2010, 09:40 AM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 05-01-2010, 10:37 AM
RE: Adhesives and Moisture - CC Solutions - 05-02-2010, 08:18 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 6,323 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 20,800 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 5,610 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 8,046 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 12,792 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 65,786 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 15,095 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 22,644 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM
17 Replies 44,206 Views
Last Post by CC Solutions
04-01-2011, 09:02 PM

Users browsing this thread:
1 Guest(s)