@WagnerMeters - Q: Just returned from meeting where cust. says they get 50% false positives with rapidrh other 50% pass, any tips to avoid?

They are having trouble getting reproducible tests. I suspect they are not using rapid rh and so their probes aren't being acclimated and calibrated properly. But if they were using rapid rh what might be the cause of this?

We don't have this problem in California with our subs who use rapid rh. But once and a while we will get one or two test sites that are off. But nowhere close to 50%.









Messages In This Thread
50% fail rate - eaadams - 05-27-2011, 10:55 AM
RE: 50% fail rate - EWagner - 05-27-2011, 03:55 PM
RE: 50% fail rate - eaadams - 05-27-2011, 04:57 PM
RE: 50% fail rate - CC Solutions - 05-30-2011, 11:18 AM
RE: 50% fail rate - eaadams - 05-30-2011, 01:24 PM
RE: 50% fail rate - CC Solutions - 09-12-2011, 05:43 PM
RE: 50% fail rate - eaadams - 09-13-2011, 03:07 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 05:44 PM
RE: 50% fail rate - eaadams - 09-13-2011, 05:50 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 05:58 PM
RE: 50% fail rate - eaadams - 09-13-2011, 06:01 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 06:04 PM

Users browsing this thread:
1 Guest(s)