#Login Register
50% fail rate
  • 0 Vote(s) - 0 Average


09-13-2011, 05:50 PM #9
eaadams Concrete Moisture Expert *****
Status: Offline Posts:596 Threads:86 Joined:Jul 2010
So you mitigate the area of the test or the whole slab with one high test?

For example patient room #206 is high, room #207 is fine, #205 is fine, and the hallway is fine. Do you just mitigate room #206?








Messages In This Thread
50% fail rate - eaadams - 05-27-2011, 10:55 AM
RE: 50% fail rate - EWagner - 05-27-2011, 03:55 PM
RE: 50% fail rate - eaadams - 05-27-2011, 04:57 PM
RE: 50% fail rate - CC Solutions - 05-30-2011, 11:18 AM
RE: 50% fail rate - eaadams - 05-30-2011, 01:24 PM
RE: 50% fail rate - CC Solutions - 09-12-2011, 05:43 PM
RE: 50% fail rate - eaadams - 09-13-2011, 03:07 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 05:44 PM
RE: 50% fail rate - eaadams - 09-13-2011, 05:50 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 05:58 PM
RE: 50% fail rate - eaadams - 09-13-2011, 06:01 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 06:04 PM