Does Wagner go to 100% (spinal tap anyone) or does it max out at 99%? I've never seen 100%.

Does ASTM allow for 100% as I see some tech data sheets that mention 100% from concrete companies.

07-12-2012, 01:40 PM #2
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,066 Threads:69 Joined:Dec 2009
The readers go to 99%.

The product design committee asked Jason if they should insert another LCD decimal place or if he wanted to spend the design money on a trip to Hawaii.... To which Jason replied: "Mahalo nui loa!"Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

07-12-2012, 02:48 PM #3
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
When the RH level exceeds 99%, the LED reads "Hi"

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

07-12-2012, 02:58 PM #4
rapidrhrep Concrete Moisture Tutor **
Status: Offline Posts:83 Threads:3 Joined:Aug 2011
@ Mr Grafton or should I address you as Sage Grafton----ALOHA!!

@ Mr Nixon: You are absolutely correct, regarding reading "Hi" on the older blue versions. When we transitioned to the orange 4.0 version, we revised the firmware to just read 99% max.

Jason

07-12-2012, 05:03 PM #5
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Thanks, Jason. Didn't know of the change. Just figured I hadn't encountered any substrates that high.